SARAMANT VS 30:
- Composition:
WC 83%, TaC/NbC 2,5%,
TiC 4,5%, Co 10%
- Density: 13,3 g/cm3
- Hardness: 1450 HV30
This grade is mainly used for higher cutting speeds
and a small chip cross section.
SARAMANT VS 50:
- Composition WC 69%, TaC/NbC 8%, TiC 5%, Co 18%
- Density: 12,4 g/cm3
- Hardness: 1220 HV30
This grade is mainly used for lower cutting speeds and a large
chip cross section.
|